Search Documents

Sort by

  • AIME
    Oxidation of Pyritic Sulphur in Coal Mines

    By Stephen Burke

    THE oxidation of pyritic sulphur associated with coal is important for the following reasons: 1. It is the predominant cause for the formation of acid mine drainage issuing from bituminous coal seams

    Jan 1, 1937

  • SME
    Oxidation of Refractory Gold Ores: A Comparison of Alternatives

    By James Whitlock, Michael Robert Wilcox

    The volume of recently published material in praise of various refractory gold ore treatment methods is impressive. The authors are unfailingly bright, focused and thorough, and as each paper conclude

    Jan 1, 1991

  • IOM3
    Oxidation of silver-copper selenide matte in copper-anode slimes smelting

    By G. G. Barbante

    The oxidation behaviour of selenide matte with a substantial Cu content and low Ag differs significantly from that of high-Ag matte. Low-Ag selenide mattes display a large oxygen solubility and the up

    Jun 19, 1905

  • TMS
    Oxidation of Synthetic Nickel Mattes Under Simulated Flash Smelting Conditions

    By Satu Jyrkönen

    A single-particle laminar-flow technique was used to study oxidation of four synthetic nickel mattes, which were screened into three size fractions, Experimental conditions were: reaction gas from N2

    Jan 1, 1996

  • AUSIMM
    Oxidation of Zinc Sulfide in a Fluidised Bed of Very Low Oxygen Concentration

    By Miyatani J. Asaki Z, Kondo Y

    The oxidation of sphalerite particles of 60 to 100 mesh size was studied in a fluidized bed of low 02 concentration at 900¦C. Par- tial pressure of 02 in the fluidizing 02-N2 gas mixture was chosen

    Jan 1, 1980

  • TMS
    Oxidation Reactions in a Dispersed Copper Smelting System

    The merging of flash smelting with spray converting in one single furnace is proposed as a continuous copper making process. The proposed process is expected to produce blister copper, clean slag and

    Jan 1, 1976

  • AUSIMM
    Oxidation Reduction Potential of Activated Carbon During Anion Loading

    By Muir DM, Tsuchida N, Dalton R

    The adsorption or loading of anions onto extruded based peat activated charcoal has been studied by potential measurements in a flow through cell. Loading rates are in the order F-

    Jan 1, 1984

  • TMS
    Oxidation Removal Behavior Of Boron And Local Nonequilibrium Reaction Field In Purification Process Of Molten Silicon By The Flux Injection Technique

    By Mitsuru Tanahashi

    Oxidation removal of boron from molten silicon by injecting oxygen and highly basic CaO-CaF2flux powder has been investigated with special attention to the dynamic behavior of the injected flux partic

    Jan 1, 2006

  • CIM
    Oxidation Resistance of Haynes® Hr-224TM Alloy

    By H. J. White

    Haynes International, a world leader in the manufacture and production of nickel, and cobalt base alloys has invented and developed a low cost high temperature material, with a unique combination of s

    Jan 1, 2010

  • SAIMM
    Oxidation state of titanium in CaO-SiO2-TiOxslags at 1873K

    By P. Gonzalez, C. Ariyo, L. Holappa

    Oxidation state of titanium was determined in CaO-SiO2-TiOxslags in the composition range25–53 per cent CaO, 27–46 per cent SiO2, 10–55 per cent TiOxat 1873K using gas equilibration method. In the

    Jan 1, 2004

  • CIM
    Oxidation, Weight Gain and Self-Heating of Sulphides

    By J. E. Nesset, J. A. Finch, Rosenblum. F., S. Somot

    "In a previous presentation at the CMP, evidence was shown for the formation of hydrogen sulphide (H2S) in self-heating experiments on pyrrhotite-rich samples (Somot and Finch, 2006). Oxidation of H2S

    Jan 1, 2009

  • AIME
    Oxidation-collection Method of Assaying Sulphide Ores for Gold and Silver

    By Orson Shepard

    TEXTBOOKS on fire assaying list the following standard methods of assaying sulphide ores: (1) scorification, (2) litharge-niter, (3) soda-iron, (4) roasting, (5) combination wet and fire. The litharg

    Jan 1, 1939

  • CIM
    Oxidation-Precipitation Method to Treat Cyanide Effluents

    By H. Soto, J. Jara, F. Nava

    "A combination of oxidation and precipitation was used to eliminate cyanide from gold milling effluents. Preliminary laboratory work developed with both synthetic cyanide solutions and with industrial

    Jan 1, 1992

  • SME
    Oxidation-Precipitation Method to Treat Cyanide Effluents (47624545-3423-4139-b9bb-ca19a5be6837)

    By H. Soto, J. Jara, F. Nava, J. B. Hiskey, B. J. Scheiner

    Laboratory tests showed that ozone can destroy free cyanide and weakly complexed cyanide (copper and zinc cyanides). The iron cyanide complexes were resilient to ozonation but they were effectively el

    Jan 1, 1993

  • SME
    Oxidation/Reduction Effects In Depression Of Sulfide Minerals

    By S. Chander

    A review of the published literature on the mechanism of depression of sulfide minerals shows that a unified theory is not yet available. The various mechanisms that have been postulated include compe

    Jan 1, 1984

  • AIME
    Oxidation/Reduction Effects In Depression Of Sulfide Minerals-A Review

    By S. Chander

    A review of the published literature on the mechanism of depression of sulfide minerals shows that a unified theory is not yet available. Various mechanisms that have been postulated include competiti

    Jan 1, 1986

  • CIM
    Oxidative Acid Leaching of a Nickel Sulphide Concentrate: Comparison of Options

    By G. Wren

    As base metal sulphide resources become increasingly challenging to process, producers seek alternative options to treat concentrates. This study considers the mineral, elemental, and leaching charact

    Jan 1, 2014

  • AUSIMM
    Oxidative combustion law of water soaked coal under oxygen-lean condition

    By H Y. Niu

    The coal left in the goaf is easily submerged by groundwater damage. During the mining process of the underlying coal seam, it is necessary to drain the water in the overlying goaf. The coal sample is

    Oct 12, 2022

  • SME
    Oxidative Destruction Of Ammonia For Restoration Of Uranium Solution Mining Sites

    By Michael J. Humenick

    A laboratory experimental research project was conducted to evaluate the use of chlorine for the oxidative destruction of residual ammonia which may remain in ground water after in-situ uranium soluti

    Jan 1, 1982

  • AIME
    Oxidative Destruction of Ammonia for Restoration of Uranium Solution Mining Sites (1fba419e-57ec-43d1-a83a-fcca552f0d9e)

    By M. J. Humenick, K. Garwacka

    A laboratory experimental research project was conducted to evaluate the use of chlorine for the oxidative destruction of residual ammonia that may remain in ground water after in-situ uranium solutio