Search Documents
Search Again
Search Again
Refine Search
Refine Search
-
Degradation Behaviour of SPS Processed Neodymia Doped Cubic YSZ in Supercritical WaterBy L. Bichler, A. Siebert-Timmer
In this research, novel YSZ ceramics doped with 5 mol% Nd2O3 were manufactured via Spark Plasma Sintering (SPS) process. The sintered Nd2O3-YSZ ceramics were subjected to a static supercritical water
Jan 1, 2014
-
The Historical Development of Electrolyte Additives and Their Specific Role and Influence on Cathode QualityBy J. Brent Hiskey
At present, approximately 80 % of the worlds mine production of copper is achieved by smelting and electrorefining. The principle aim of copper electrorefining is to satisfy the large demand for extre
Jan 1, 2019
-
Federal budget disappointsBy Robert B. Parsons
"Finance Minister Paul Martin's first budget disappointed almost everyone. The business sector was disappointed at the some what feeble attempt to grapple with the country's deficit. The min
Jan 1, 1994
-
Continuous Gas Holdup Measurement in Flotation ColumnsBy R. Pérez, James A. Finch, F. Tavera, Cesar O. Gomez
"Gas holdup is a variable which affects the operation of flotation columns. On one hand, gas holdup is a function of bubble size (a function of sparger type, frother characteristics and concentration,
Jan 1, 1995
-
Design and R&D Progress of China’s Largest Underground Nonferrous Mine—Pulang Copper MineBy Zhang Wei
"Pulang Copper Mine is located in Shangri-La county, Diqing Prefecture, Yunnan Province, with currently defined copper reserve of 4.8 million tonnes of copper metal and an average grade of 0.34% Cu. T
Jan 1, 2016
-
A Best Practice Database for Energy Management Initiatives in the Mining IndustryBy M. Y. Levesque
The Australian Government?s Energy Efficiency Opportunities (EEO) program launched in 2006 obliges companies that use more than 0.5 PJ (petajoule) or roughly 139 GWh (gigawatt hour) per year to conduc
Aug 1, 2013
-
The Effect of Water Chemistry, Reagent Type, and Other Environmental Factors on the Performance of Industrial Grinding and Flotation Processes Involving Sulfide MineralsBy Richard R. Klimpel
"This paper discusses the effect of water chemistry, reagent type, and other environmental factors on the performance of sulfide mineral size reduction and froth flotation processes. Two specific prob
Jan 1, 1996
-
Further Notes Concerning Ore-ShootsBy G. Vibert Douglas
Introduction A preliminary paper dealing with the subject of ore-shoots was presented to this Society at its Annual Meeting last year (1). The present paper records the attempts which have been made
Jan 1, 1935
-
Permitting, Construction and Commissioning of a New Slag Landfill at Boliden HarjavaltaBy Esa Peuraniemi, Hanna-Leena Heikkilä
Boliden Harjavalta has been operating a copper flash smelter since 1949. Thus, in 2019, the smelter is celebrating its 70th anniversary of flash smelting. Slag formation is an integral part of the sme
Jan 1, 2019
-
Relationship of Structure to Ore Deposition at the Britannia MinesBy Frank Ebbutt
Introduction The property of the Britannia Mining and Smelting Company, Limited, is situated on the east side of Howe sound, about six miles from its head. It is roughly thirty miles by water from Va
Jan 1, 1935
-
Austin Gold Venture Bioleaching: Project SummaryBy J. Kuipers, R. W. Lawrence, P. B. Marchant, W. Brooks, J. T. Chapman
"Bioleach testing and piloting was conducted on refractory gold sulphide concentrate from Austin Gold Venture in Nevada during 1988. The objective of the test programme was to determine the technical
Jan 1, 1989
-
Strength Characteristics of Paste Fill Prepared with Agglomerated Fine Tailings PelletsBy Laxman M. Amaratunga, David N. Yaschyshyn
"In the mining industry several types of fills are used for backfill operations. They are broadly categorized into three basic types: rock fill, hydraulic/slurry fill, and paste fill. Recently, paste
Jan 1, 1996
-
East Boulder Mine - A River Runs Through ItBy Ken J. Brouwer
Stillwater Mining Company commenced construction and development of the East Boulder underground mine in 1998. This new PGM mine is situated adjacent to the East Boulder River approximately 35 miles s
May 1, 2002
-
TPH/Cubic Metre - An Alternative View on High Density Thickener Design & GeometryBy David Minson
On many occasions, operators have seen that high density and paste thickener performance does not meet the initial design expectations, and the installed equipment produces lower than expected thicken
Jan 1, 2019
-
Stress Measurement: The GRC PerspectiveBy N. Bahrani
Knowledge of the state of stress in the Earth?s crust is very important to the safe and efficient development of underground excavations in mining and civil engineering projects. A number of methods h
Aug 1, 2013
-
Continuous Casting of Az31 Magnesium Plate via Horizontal Continuous Casting ProcessBy Bong Sun You
AZ31 magnesium plate of 300mm in width and 40mm in thickness was produced by horizontal continuous casting machine, and its microstructures were analyzed on the surface and in the plate interior. The
Jan 1, 2006
-
Selen-IXtm: Selenium Removal from Mining Affected Runoff Using Ion Exchange Based TechnologyBy A. West, F. Mohammadi
Growing awareness of selenium bioaccumulation has resulted in selenium management becoming an important environmental issue for mining operations. Selen-IX™ is a novel ion exchange based technology de
Jan 1, 2014
-
Risk Simulation of Aquifer CO2 Disposal from Thermal Power PlantsBy Samuel Frimpong
Green house gases have become a major concern within the international community over the last two decades due to their potential link to global warming. Carbon dioxide (CO2) is the principal greenhou
May 1, 2001
-
FEM analysis of plastic deformation in Brinell hardness testing: correlation between strength and hardness in aluminum alloysBy S. Maleksaeedi
On-site evaluation of strength using hardness is common for different materials. The lack of such relation for aluminum alloys has always been felt. In this work, a finite element analysis of plastic
Jan 1, 2004
-
Dissolution of AlTiSi intermetallic compounds in A356 Al-Si alloyBy A. Jafarnia
Aluminum alloys are frequently grain refined during solidification in order to promote the formation of an equiaxed grain structure in the casting. The application of Ti-based grain refiners and/or Ti
Jan 1, 2004