Oxysulphide in Metallurgy of Nickel and ColbaltBy I. D. Reznik
On blowing nickel matte in a converter without quartz, first the oxidation of metallic iron and a part of FeS occurs without evolving sulfur dioxide, the formed FeO dissolves in a sulphide smelt and f
Jan 1, 1997
-
A Laboratory Investigation of the Reduction of the Iron Carbonate Bearing Ore to Iron Nugget by Means of the ITmk3 TechnologyBy R. S. Tahautdinov, A. N. Posazhennikov, V. V. Bastrygin
"The Bakal (South Ural, Russia) deposit of iron ore bearing iron carbonate (siderite) with the capacity of more than 1 billion tones belongs to the MMK. This ore cannot be fully processed via blast fu
Jan 1, 2011
-
A Laboratory Investigation of the Reduction of The Siderite Iron Ore to Iron NuggetBy E. V. Redin
"The Bakal (South Ural, Russia) deposit of iron ore bearing iron carbonate (siderite) with the capacity of more than 1 billion tones belongs to the MMK. This ore cannot be fully processed via blast fu
Jan 1, 2012
-
Arsenic Control in the Sulfuric Acid Plant by the Purification System of Caraiba MetaisBy Esther Carrera Martinez
Caraiba Metals is the sole brazilian copper custom smelter. The sulfur present in the various concentrates processed is recovered as sulfuric acid and oleum ,which are sold in the local market For qua
Jan 1, 1996
-
Modelling of Sulphide Capacities of Some Silicate MeltsBy R. Nilsson
In the present work, an assessment of the sulphide capacities of a number of binary and ternary slag systems have been carried out in the light of a sulphide capacity model. The model is based on the
Jan 1, 1996
-
Hypochlorite Pretreatment of a Low Grade Carbonaceous Gold Ore, Part II: Effects of Agglomeration, Temperature and Bed HeightBy Mojtaba Ahmadiantehrani
A previous study showed that up to 80% gold extraction could be obtained with 160 lbs/ton hypochlorite consumption at ambient temperature from a low grade Carlin-type carbonaceous ore. Crushing the or
Jan 1, 1992
-
Current Operation at La Caridad SmelterBy J. H. Meza V
La Caridad operated at only 65% of design capacity during the first five years of operation. After the first major shutdown and repairs to the furnace in mid- 1992, the smelter quickly reached 95% of
Jan 1, 1993
-
Effects Of Mineral Oxides On The Precipitation Micro-Morphology Of Metallic Iron In The Reduction Of Iron Oxides Under Co AtmosphereBy ZhiLong ZHAO, Lin Lin, Zhancheng Guo, Jingtao GAO, Huiqing Tang
Grain sticking often occurs in the fluidized bed reduction of f ine iron ore, which is closely related to the precipitation morphology of metallic iron on the surface of ore particles. In this work, s
Jan 1, 2016
-
INCO?s Procedure For Controlling Warpage in Copper Moulds used for Anode CastingBy R. A. Roberti
Most copper refineries use conventional wheel systems to cast anodes. over a period of time the copper moulds that are used become warped and cracks develop. To control mould warpage, the mould's
Jan 1, 1987
-
Handling of Slags Leaving Metallurgical VesselsBy J. S. Pitsillos
A new furnace tapping technique involving the simulation of a control valve at the exit to a furnace is being investigated. The purpose of this new tapping technique is to regulate the flowrate of liq
Jan 1, 1991
-
Synthesis. Characterization And Ion Exchange Of New Na / Nb / M4+/ O / H2O (M = Ti, Zr) PhasesBy May Nyman
Due to the vast diversity of chemical media in which metal separations are executed, a wide range of ion separation materials are employed, This ,results in an ongoing effort to discover new phases wi
Jan 1, 1999
-
Recycling Of Li/soci2 Battery WastesBy Arpad E. Tonna
Recycling of materials from lithium-oxyhalide batteries is a complex task, since the dismantling of batteries is associated with many hazards. The electrolyte and the lithium anode metal are extremely
Jan 1, 1995
-
Charactarisation of Corrosion Properties of Za-27/ Quartz Metal Matrix CompositesBy Uchil Jayagopal, P. V. Krupakara, S. Manjunath
"This paper deals with the corrosion characterization of quartz particlate ZA-27 alloy metal matrix composites (MMCs). Quartz particles of size 50-80 microns are used as reinforcement. MMC's are prepa
Jan 1, 2000
-
Electrodeposition of Cobalt from Air and Water-Stable Ionic Liquid 1-Butyl-3-Methylimidazolium TetrafluoroborateBy Zhao wen Wang, Ramana G. Reddy, Min Li
"The electroreduction of Co(II) in l-butyl-3-methylimidazolium tetrafluoroborate (BMlMBF4) ionic liquid was investigated by cyclic volatrnmetry at 353 K. The results show that the reaction of Co(II) t
Jan 1, 2014
-
Recycling Of Used Aluminum Beverage Cans In JapanBy Tatsuo Itou
Both sales volume of Aluminum Can and its recycling rate are remarkably increasing here in Japan. In 1993, recycled can volume was 11.78 billion cans ( 116,258 metric tons ) and its recycling rate
Jan 1, 1995
-
Effect Of Pressure On The Corrosion Of Materials In High Temperature WaterBy Sheng-li Wu, Guo-liang Zhang, Bo Su
One of the major challenges for the Canadian Gen IV Super-Critical Water-cooled Reactor (SCWR) concept is the selection of fuel cladding materials. The Canadian SCWR concept will operate at a core out
Jan 1, 2015
-
The Use of Inorganic Peroxides as Accelerators for Gold Heap LeachingBy S. P. Ball
A major limitation to maximising the rate of gold extraction in commercial operations occurs as a consequence of the limited solubility of oxygen in cyanide liquors. The use of additions of solid inor
Jan 1, 1989
-
Ladle Metallurgy Kinetics: Inclusion-Inclusion ReactionsBy P. Chris Pistorius
An example is presented to illustrate the joint effect of local reaction equilibria and mass transfer limitations, for reactions during ladle refining of steel. The example relies on some of the kinet
Jan 1, 2014
-
The Role of Arsenic Minerals in the Recovery of Platinum-Group Elements from Gabbroic RocksBy I. Iwasaki
Platinum group elements (PGE) are often found in arsenide and sulfarsenide minerals as inclusions in copper-nickel bearing gabbroic rocks. Major losses of platinum in flotation have been attributed to
Jan 1, 1988
-
Photo-catalytic, Semiconducting and Ion Conducting Properties of AgCuS Film on ChalcopyriteBy Charles L. Richman
The effect of the addition of Silver Sulfide on the rate of Chalcopyrite (CP) of Sulfuric acid (H2SD4 leaching is discussed, Although Ag2S in an expensive addition, a theoretical explanation of it&apo
Jan 1, 2001