Leaching Behavior of the Roasted Nickel CalcineBy D. Yu, T. A. Utigard, M. Barati
"Sulfation roasting of nickel concentrate to generate water-soluble metal sulfates was investigated as an alternative process to smelting for the recovery of valuable metals. The kinetics of dissoluti
Jan 1, 2012
-
Leaching Behaviour and Metal Fixation Within Cemented Paste Backfill MaterialsBy E. Fried
Cemented paste backfill (CPB) is an innovative tailings management method that consists in returning considerable amounts of mine tailings into the underground mine openings. The filled stopes thus pa
May 1, 2007
-
Leaching Behaviour And Particle Interactions In Uranium Laterite Dispersions: Effect Of Ore Mineralogy And TemperatureDue to complex mineralogical and chemical interactions of the value and gangue mineral phases present in uranium-containing lateritic ores, deleterious pulp gelation which impacts on value metal recov
Sep 1, 2012
-
Leaching Behaviour of a Colombian Nickel Laterite in Aqueous Alkaline Glycine SolutionsBy G. T. Lapidus, A. Garcés, O. J. Restrepo
"Colombian nickel laterites have historically been processed by pyrometallurgy. However, due to the depletion in ore grades, alternative processes are required. Hydrometallurgical processes, such as p
Jan 1, 2017
-
Leaching Characteristics of a Low-Grade Nickel-Bearing Ore Upgraded on the Falcon ConcentratorBy M. B. Shongwe, R. K. K. Mbaya, C. K. Thubakgale, P. Mendonidis
"A low-grade nickel-bearing ore was pre-concentrated on a SB40 laboratory model Falcon Concentrator. Three size fractions, -212+125, -125+75 and -75 µm were tested with the intent to upgrade the nicke
Jan 1, 2017
-
Leaching Characteristics of Australian Uranium OresThe leaching characteristics of a number of Australian uranium ores were determined under acid and alkaline conditions. Ores from the Ranger, Nabarlek and Koongarra deposits in the Northern Territory
Jan 1, 1979
-
Leaching characteristics of cerium and yttrium from non-magnetic coal fly ash after silicate digestion using acetic acidBy H. Manurung, I. M. Bendiayasa, W. Astuti, and H. T. B. M. Petrus, F Anggara, K. C. Wanta
The leaching kinetics of cerium (Ce) and yttrium (Y) in sodium-hydroxide-digested non-magnetic coal fly ash using acetic acid were investigated. The variables analysed were pH, solid-to-liquid ratio (
Nov 6, 2024
-
Leaching Characteristics Of Copper Refractory Ore In Sulfate MediaRefractory copper ores (CROs) in central Africa contain copper minerals that are locked up in a micacious solid matrix or associated with carbonate, sulfide and phosphate minerals. Several researchers
Jan 1, 2011
-
Leaching Characteristics Of Copper Refractory Ore In Sulfate Media (72fefa33-b60e-41f5-b286-1b56b05d7e4d)Refractory copper ores (CROs) in central Africa contain copper minerals that are locked up in a micacious solid matrix or associated with carbonate, sulfide and phosphate minerals. Several researchers
Nov 1, 2011
-
Leaching characteristics of heavy metals from three historical Pb-Zn mine tailings heaps in the United KingdomBy G. Merrington, B. J. Alloway
Tailings from three historical mining areas in the UK were leached in columns under a simulated weathering programme which was chosen to represent periods of 1 and 2 years at 3 different ambient tempe
Jan 8, 1993
-
Leaching Characteristics of Nickeliferous Pyrrhotite Tailings from the Sudbury, Ontario AreaBy Elizabeth Edwards, Radhakrishnan Mahadevan, Vladimiros G. Papangelakis, Srinath Garg, Kurtis Judd
Mineralogical characterization of the tailings showed the deportment of Ni to be similar in the Vale and Glencore tailings, with 60% of the total Ni locked in pyrrhotite, and the balance 40% associate
Jan 1, 2017
-
Leaching Complex Gold OresCalaverite is a gold telluride found in the Kalgoorlie region, Fiji, Cripple Creek Colorado and numerous other locations. It is known that a high pH is necessary for calaverite cyanidation, with the l
Jan 1, 2014
-
Leaching Concentrates without Leaching IronBy M. Maccagni, J. Nielsen
"Engitec developed the EZINEX® Technology some years ago to recover zinc from oxidized secondary sources. This process works at neutral pH and can take into solution any kind of metal, but iron is re
Jan 1, 2016
-
Leaching Copper from Worked-Out Areas of the Ray Mines, ArizonaBy Robert W. Thomas
LEACHING of mined-out areas at the Arizona property of the Ray Mines Division, Kennecott Copper Corp., was started on Jan. 20, 1.937, and by July 1, 1938, 10,000,000 lb. of copper had been produced by
Jan 1, 1938
-
Leaching Kinetics And Mechanisms Of Surface Reactions During Cyanidation Of Gold In The Presence Of Pyrite Or StibniteBy A. Pratt, G. Deschênes
This paper quantifies the detrimental effects of pyrite and stibnite on gold leaching kinetics. Means to reduce the effect of these minerals by addition of lead nitrate and oxygen are presented. A sig
Jan 1, 2004
-
Leaching Kinetics of Iron in Atmospheric Direct Leaching of MarmatiteBy H. Zhu, Q. Jiang
The leaching kinetics of iron during the atmospheric direct leaching (ADL) of marmatite concentrate was studied under the following conditions: reaction temperature of 343-383 K, slurry pressure of 0.
Jan 1, 2014
-
Leaching Kinetics of Rare-Earth Elements from Complex Ores by Acidic SolutionsBy Eren Hüseyin Obuz
In this study, the leaching kinetics of rare-earth elements were investigated using HCl and HNO3 solutions. A standard crushed complex ore was utilized as raw material. The complex ore (particle size
-
Leaching Kinetics Study Of The Mehdi-Abad Low Grade Zinc Oxide OreBy B. Hosseini
Considering the subtractive trend of the sulfide and high-grade zinc ores in worldwide and also in Iran, Nowadays special attentions have been drawn to the extraction of zinc from its other resources
Sep 1, 2012
-
Leaching Mechanism of Complicated Antimony- lead Concentrate in Slurry ElectrolysisBy C. Y. Wang
Anodic reaction mechanism of complicated antimony-lead concentrate in Slurry Electrolysis has been investigated by the anodic polarization curves determined under various conditions. The main reaction
Jan 1, 2014
-
Leaching of a Gold Ore Using the Hydrogen Sulfide-Bisulfide-Sulfur SystemBy P. West-Sells, B. Wassink, N. Fisher
Gold leaching from a commercial cyanide-amenable gold ore was studied at 25°C using sodium bisulfide-hydrogen sulfide solutions containing elemental sulfur. Gold extraction from the ore using 0.55 M N
Jan 1, 2005