    The tailings dusting problem: a case study of mining operations in the Far North of the Russian Federation, D.V. Makarov, A.V. Svetlov, E.A. Krasavtseva, O.T. Konina, A.A. Goryachev, and V.A. Masloboev

    By O. T. Konina, V. A. Masloboev, A. V. Svetlov, E. A. Krasavtseva, D. V. Makarov, A. A. Goryachev

    Dusting phenomena have been examined at the tailings storage facility of Apatit JSC Kirovsk, a mining operation located in the far north of the Russian Federation. The material composition of the tail

    Jan 1, 2020

  • SAIMM
    Chemical And Physical Changes Of Cathode Carbon By Aluminium Electrolysis

    By J. Hop, A. Støre, T. Foosnæs

    The carbon cathode for aluminium electrolysis is also part of the container of the process. In order to understand the behaviour and possible failure of the cathode, detailed material properties under

    Jan 1, 2004

  • SAIMM
    Introducing new Council members (8abfb381-4e73-40b7-9db7-58d2171c5e01)

    Mr K.R. Beard was born on 19th December, 1958. He attended Marist Brothers College, Observatory, and Marist Brothers College, Linmeyer. He was awarded a bursary by SEIFSA (Steel and Engineering Indu

    Jan 1, 1989

  • SAIMM
    Viscosity and flow behaviour of TiO2-containing blast furnace slags under reducing conditions

    By Y. Mao, D. Xie

    The viscosity of TiO2-containing blast furnace slags may increase rapidly (commonly referred to as thickening) under strong reducing conditions in the blast furnace. To elucidate the mechanisms for sl

    Jan 1, 2004

  • SAIMM
    Thermodynamic Investigations Of Corrosion Phenomena Caused By Metal Halide Salt Melts In High Temperature Discharge Lamps

    By T. Markus, K. Hilpert

    Discharge vessels of advanced light sources are made of translucent polycrystalline Al2O3(PCA).These tubes contain salt mixtures, which essentially consist of metal halides. The salt mixture is presen

    Jan 1, 2004

  • SAIMM
    Electro Smelting Of Ilmenite For Production Of TiO2 Slag - Potential Of India As A Global Player

    By S. Asokan, CVGK Murty, R. Upadhyay

    The principal mineral sources of titanium are rutile, anatase (both TiO2), ilmenite (FeTiO3) and leucoxene (a weathered ilmenite of variable concentration of TiO2 but similar to pseudorutile Fe2Ti3O9)

    Jan 1, 2007

  • SAIMM
    Large-Scale Design And Testing Of An Improved Fine Coal Dewatering System ? Synopsis

    By M. Le Roux

    Fine coal (-500 µm) is notoriously difficult to dewater. It is not uncommon for a dewatered product to have a moisture content as high as 30 per cent after vacuum filtration. This poses several handli

    Jan 1, 2012

  • SAIMM
    Slag Properties And Design Issues Pertinent To Matte Smelting Electric Furnaces

    The effect of composition on electrical conductivity (resistivity), viscosity and liquidus temperature of the slags encountered in electric smelting of PGM containing suphide concentrates is reviewed,

    Jan 1, 2004

  • SAIMM
    Bateman Mega DMS Modules- Successes And Challenges - Introduction

    By N September, R Abate

    Bateman Modular (previously Van Eck and Lurie) has been building and supplying the mining industry with modular DMS plants for the last 30 years. These DMS modules range in capacity from 1 tph to 200

    Jan 1, 2006

  • SAIMM
    Large-Scale Design And Testing Of An Improved Fine Coal Dewatering System - Synopsis (0b7ce52d-2bd9-4f5e-84a7-9ce2b2e08562)

    By M. Le Roux

    Fine coal (-500 µm) is notoriously difficult to dewater. It is not uncommon for a dewatered product to have a moisture content as high as 30 per cent after vacuum filtration. This poses several handli

    Jan 1, 2012

  • SAIMM
    Interactions Of Two-Liquid CaO-MgO-FetO-P2O5 Slag With MgO Refractories

    By T. Tamura

    It is known that the CaO-FetO-P2O5slag system has a wide liquid miscibility gap at steelmaking temperatures and this two-liquid slag phase has many advantages such as high activities of both FetO and

    Jan 1, 2004

  • SAIMM
    Liquidus temperature and viscosity of melter slags

    By M. Somerville, S. Sun

    The liquidus temperature and viscosity of a range of melter slags produced in South Africa were determined. Drop-quench experiments were carried out on the supplied plant samples to determine the liqu

    Jan 1, 2004

  • SAIMM
    Slags In Ferroalloys Production - Review Of Present Knowledge

    By L. Holappa

    Ferroalloys like FeCr and FeMn are mostly produced in submerged electric arc furnaces. Typical for these processes is that the amount of slag is quite high. The role of slag for the process is thus ve

    Jan 1, 2004

  • SAIMM
    Physico-chemical properties and transition metal complex formation in alkali pyrosulphate and hydrogen sulphate melts

    By H. Hamma, R. Fehrmann, M. Gaune-Escard, G. Hatem, S. B. Rasmussen, K. M. Eriksen

    The molten salts M2S2O7and MHSO4, the binary molten salt systems M2S2O7-MHSO4and the molten salt-gas systems M2S2O7-V2O5and M2S2O7-M2SO4-V2O5(M = Na, K, Rb, Cs) in O2, SO2and Ar atmospheres have been

    Jan 1, 2004

  • SAIMM
    Thermodynamic Modelling Of The Al2O3-CaO-CoO-CrO-Cr2O3-FeO-Fe2O3-MgO-MnO-NiO-SiO2-S System And Applications In Ferrous Process Metallurgy

    By A. D. Pelton, Y. -B. Kang, S. A. Decterov

    Computerized thermodynamic databases for solid and liquid metal, slag and solid oxide phases in the Al2O3-CaO-CoO-CrO-Cr2O3-FeO-Fe2O3-MgO-MnO-NiO-SiO2-S system have been developed by critical evaluati

    Jan 1, 2004

  • SAIMM
    Rock mass defect patterns and the Hoek-Brown failure criterion

    By S. Read, G. Cook

    The Hoek-Brown failure criterion is often applied to a wider range of rocks than the isotropic rock masses to which it is strictly applicable. This paper evaluates the patterns of defects in rock mas

    Jan 1, 2003

  • SAIMM
    Experimental Model Study For Separation And Dissolution Of Liquid Inclusions At The Interface Between Steel And Slag

    By M. Magnelöv, Du Sichen, U. Sjöström

    An experimental study has been performed to investigate the behaviour and separation of inclusions at the interface between steel and slag. The study has been limited to liquid inclusions because they

    Jan 1, 2004

  • SAIMM
    The Use Of Low-Toxic Heavy Suspensions In Mineral Sands Evaluation And Zircon Fractionation

    By Stafford McKnight, Larissa Koroznikova, Steve Hall, Cameron Klutke

    This paper outlines a simple methodology for mineral characterisation, developed as part of the Australian Mineral Industry Research Association (AMIRA) managed research project P777 ?The Development

    Jan 1, 2007

  • SAIMM
    Quasi-chemical viscosity model for fully liquid slags in the A12O3-CaO-‘FeO’-SiO2system

    By A. Kondratiev

    A structurally-based viscosity model for fully liquid silicate slags has been developed and applied to the Al2O3-CaO-‘FeO’-SiO2system at metallic iron saturation. The model links the slag viscosity to

    Jan 1, 2004

  • SAIMM
    Activity of chromium oxide in CaO-SiO2based slags at 1873 K

    By K. Morita, N. Sano

    Thermodynamic properties of chromium oxides in molten slags are very important for optimization of stainless steel refining processes as well as reduction processes of chromium ores. The solubility of

    Jan 1, 2004