Abstract

High melting point inclusions, such as spinel, alumina and AlO rich calcium-aluminates, have a strong tendency to agglomerate on the tundish stopper rod and Submerged Entry Nozzle (SEN) during the steel casting process, and eventually to cause SEN clogging. Calcium treatmen by wire injection during steel refining during Ladle Metallurgy (LM) is commonly used to modify these troublesome inclusions to lower melting point inclusions. However, too much Ca injection (Ca over-treatment) can cause operational issue (e.g. slide gate plate erosion),as well as increase Ca cost. Therefore, it is desirable to add an appropriate amount of Ca to avoid either under-or over-treatment. Based on inclusion analysis with an ASPEX® computer controlled scanning electron microscope (ASPEX) instrument, AlO and AlO rich calcium-aluminates were identified as a major cause of SEN clogging at ArcelorMittal Dofasco Electric Arc Furnace (EAF) steelmaking stream. A Ca treatment index was developed to improve the inclusion modification. The improved inclusion control has reduced SEN clogging and enhanced steel quality.
Citation

APA: S. Sun S. Waterfall N. Strobl D. Liao D. Holdridge  (2017)  Inclusion Control with Ca Treatment to Improve Castability of Low Carbon Aluminum-Killed Steel

MLA: S. Sun S. Waterfall N. Strobl D. Liao D. Holdridge Inclusion Control with Ca Treatment to Improve Castability of Low Carbon Aluminum-Killed Steel. The Minerals, Metals and Materials Society, 2017.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account